Thermal and catalytic cracking
- Created by: scarletto_266
- Created on: 13-01-20 09:30
Fullscreen
- Catalytic cracking
Conditions:
- Low temperature: 500 degrees celcius
- Slight pressure
- Zeolite catalyst (silicon dioxide and aluminum - with a honeycomb structure that has a very large surface area. This is done in laboratory conditions by passing long chain hydrocarbons over an aluminium oxide catalyst:
This form of…